- Hardness
- 40–90 Shore A
- Temperature
- −40 … +150 °C
- Hot water & steam
- Ozone & weathering
- Brake fluid (glycol)
Not resistant to mineral oils and fuels.
Elastomer Molded Parts · Consulting · Manufacturing
The table shows typical values. Which compound suits your application depends on media, temperature profile, load and required certificates — exactly what we clarify together.
Not resistant to mineral oils and fuels.
Sensitive to ozone and weathering.
Considerably more expensive than NBR.
Limited low-temperature flexibility; PFAS-relevant.
Low tear strength, not for fuels.
Low mechanical strength; PFAS-relevant.
Moderate oil resistance.
Not resistant to oil or ozone.
Hydrolysis in hot water.
| Code | Material | Hardness (Shore A) | Temperature | Strength |
|---|---|---|---|---|
| EPDM | Ethylene propylene diene rubber | 40–90 | −40 … +150 °C | Hot water & steam |
| NBR | Nitrile butadiene rubber | 40–90 | −30 … +100 °C | Mineral oils & greases |
| HNBR | Hydrogenated nitrile rubber | 50–90 | −30 … +150 °C | Oils at high temperature |
| FKM | Fluoroelastomer | 60–90 | −20 … +200 °C | Fuels & oils |
| VMQ | Silicone rubber | 20–80 | −60 … +200 °C | Wide temperature range |
| FVMQ | Fluorosilicone rubber | 40–80 | −60 … +175 °C | Fuels at low temperature |
| CR | Chloroprene rubber | 40–90 | −40 … +100 °C | Weathering & ozone |
| NR | Natural rubber | 30–90 | −50 … +70 °C | High elasticity |
| PUR | Polyurethane elastomer | 60–95 | −30 … +80 °C | Extremely wear resistant |
Typical values · continuous service temperature · depend on compound and media · no guaranteed properties